After fibreglass and primer coat

Gestartet von Ronald
1 Antworty 2 gefällts 0 Follower Letzte Aktivität: vor 8 Jahren
#2

After fibreglass and primer coat

Hi Ron, mark the 'real' waterline, the LWL (Load Waterline) as on your plan. Then load the boat (in the domestic Test Tank😉) down to that line then you know what she can carry, including any missing deck and superstructure of course!
See test I just did for my fish cutter 'Gina 2'.
Cheers, Doug 😎
PS: seal and prime the hull when you wish, I do final finishing / polishing when all major internal works are done, and especially after prop shaft tubes and rudder stock are fitted and 'fettled in'.
Cheers, Doug 😎
PS Applies just as well to renovations and new builds!
BUT more power to your elbow for scratch building 👍
Young at heart 😉 Slightly older in other places.😊 Cheers Doug
Gefällt von Ronald and Donnieboy
#1

After fibreglass and primer coat

So, the hull has been fibreglassed, and several coats of primer applied. What next?

Mark the water line as seen on the PDF and photographs?
OR
Place model in water, load up with approximately the weight of servos, batteries, and other building materials?

Paint exterior hull or wait till interior servos are mounted?

Scratch building questions...

Anmelden zu diesem Thread beizutragen.

Delete this post?

Es wird von der Seite entfernt.

Diesen Entwurf verwerfen?

Ihr Entwurf wird gelöscht und kann nicht wiederhergestellt werden.

Sie haben einen unvollendeten Entwurf

Was möchten Sie damit tun?